Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Total PSI 935E Polystyrene Polystyrene 935E is a high impact polystyrene exhibiting exceptional toughness for sheet and thermoforming applications.This polymer is an excellent choice for cups, food packaging, custom sheet and.. |
|||
Falling Dart Impact | 16.9 J | 12.5 ft-lb | |
Total PSI 940E Impact Polystyrene Description: 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.Applications: The combination of high gl.. |