Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 4.40 - 12.5 J
3.25 - 9.22 ft-lb
Average value: 7.66 J Grade Count:5
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..