Polymer Property : Falling Dart Impact = 11.67 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 15.82 J
11.67 ft-lb
ASTM D3029
Total PSI 945 Polystyrene
Polystyrene 945 is designed for injection molding applications requiring superior toughness. This polymer is a high impact polystyrene with excellent gloss and falling dart properties. The impact an..