Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 11.0 J | 8.11 ft-lb | ASTM D3763 |
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |