Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 0.447 J | 0.330 ft-lb | ASTM D3029 |
Total 620 Polystyrene
(discontinued **) Polystyrene 620 is an impact polystyrene designed for high gloss cap layers. The polymer has been specifically designed for co extrusion processing to produce a ductile sheet with an extremely high .. |