Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | >= 0.488 J @Temperature 23.0 °C |
>= 0.360 ft-lb @Temperature 73.4 °F |
Internal |
AKG Polymers Vision PP PPH BL1303 G30 Polypropylene Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |