Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 49.0 - 80.2 J @Temperature -40.0 - 0.000 °C |
36.1 - 59.2 ft-lb @Temperature -40.0 - 32.0 °F |
Average value: 55.4 J Grade Count:2 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Dart Drop, Total Energy | 49.0 - 80.2 J @Thickness 3.20 - 3.20 mm |
36.1 - 59.2 ft-lb @Thickness 0.126 - 0.126 in |
Average value: 55.4 J Grade Count:2 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |