Polymer Property : Dart Drop, Total Energy = 51.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
SABIC Method
SABIC Innovative Plastics Lexan® FL903 PC
Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized.
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
SABIC Method
SABIC Innovative Plastics Lexan® FL900 PC (Asia Pacific)
Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance excellent impact, flexural strength/rigidity. UL94 V-1 at .157"" (3.99 mm).
Dart Drop, Total Energy 51.0 J

@Temperature 23.0 °C
37.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FXM123R PC (Asia Pacific)
FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package ..
Dart Drop, Total Energy 51.0 J

@Temperature 23.0 °C
37.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FXM123R PC (Europe-Africa-Middle East)
FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package ..
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
SABIC Method
SABIC Innovative Plastics Lexan® FL900 PC
Lexan* resin FL900 is a Br- & Cl-free flame retardant grade that can be foamed for weight reductions. UL-94 V1 listed at 3.9mm together with good stiffness, heat, creep and impact performance make i..
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics NORYL SE1X PPE+PS (Asia Pacific)
PPO+PS. Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 244F HDT.
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific)
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific)
LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS
LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral.
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
0.1 in thick, 15 mph; ASTM D1822
Styron CALIBREâ„¢ IM 401-18 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
0.125 in, 8000 ipm; ASTM D3763
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate
EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l..
Dart Drop, Total Energy 51.0 J
37.6 ft-lb
Peak Energy; ASTM D3763
Diamond Polymers DIAMALOY PC 1812 Impact Modified Polycarbonate
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.