Polymer Property : Dart Drop, Total Energy = 50.8 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 50.8 J
37.5 ft-lb
3.39 m/sec; ASTM D3763
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Resin
Overview: CALIBREâ„¢ IM 401-18 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi..