Dart Drop, Total Energy 39.3 - 57.0 J
29.0 - 42.0 ft-lb
Average value: 49.1 J Grade Count:3
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Dart Drop, Total Energy 39.3 J

@Temperature 22.8 °C
29.0 ft-lb

@Temperature 73.0 °F
ASTM D3763
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow
Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.