Polymer Property : Dart Drop, Total Energy = 25.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 33.9 J
25.0 ft-lb
Instrumented; ASTM D3763
Westlake Plastics Tempalux® 5000 Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high heat resistance, high strength at elevated temperatures, hi..