Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 264 J | 195 ft-lb | BASF |
BASF Ultramid® BU50I PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme .. |