Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 24.4048 - 24.4048 J @Temperature -40.0 - -40.0 °C |
18.0000 - 18.0000 ft-lb @Temperature -40.0 - -40.0 °F |
Average value: 24.4 J Grade Count:1 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Dart Drop, Total Energy | 24.4048 - 24.4048 J @Temperature -20.0 - -20.0 °C |
18.0000 - 18.0000 ft-lb @Temperature -4.00 - -4.00 °F |
Average value: 24.4 J Grade Count:1 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |