Mechanical Properties Metric English Comments
Dart Drop, Total Energy 100 - 140 J
73.8 - 103 ft-lb
Average value: 130 J Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..