Polymer Property : Dart Drop, Total Energy = 14.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 8.00 - 14.0 J
5.90 - 10.3 ft-lb
Average value: 10.9 J Grade Count:7
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..