Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 910 MPa @# of Cycles 1.00e+7 |
132000 psi @# of Cycles 1.00e+7 |
Smooth (Kt = 1); Stress Ratio = 0.1; Axial Loading |
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4984 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4984.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |