Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 59.0 MPa @# of Cycles 1.00e+6 |
8560 psi @# of Cycles 1.00e+6 |
1 Hz |
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |