Fatigue Strength 790 MPa

@Diameter 25.0 mm,
# of Cycles 1.00e+8
115000 psi

@Diameter 0.984 in,
# of Cycles 1.00e+8
smooth, rod
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy;