Fatigue Strength 772 MPa

@# of Cycles 1.00e+7
112000 psi

@# of Cycles 1.00e+7
R.R. Moore Test, Smooth Rotating Beam
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..