Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 510 MPa

@# of Cycles 2.00e+6
74000 psi

@# of Cycles 2.00e+6
R=smin/smax=0.1;RT; 50% probability of failure
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Fatigue Strength 510 MPa
74000 psi
Endurance Limit (Unnotched)
Meehanite K-405 Austempered Ductile Iron
Type K-405 is for applications involving wear and requiring high tensile and endurance limit. Excellent founding properties enable more accurate castings with savings in machine stock required. Da..