Polymer Property : Fatigue Strength = 72100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 497 MPa

@Strain 0.200 %
72100 psi

@Strain 0.200 %
R=smin/smax=0.1; 2 million cycles, F50
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..