Mechanical Properties Metric English Comments
Fatigue Strength 65.0 MPa

@# of Cycles 1.00e+6
9430 psi

@# of Cycles 1.00e+6
1 Hz
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex