Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 427 MPa | 61900 psi | High cycle unnotched |
CMW® 3000 AMS-T-21014 AMS-7725 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |