Mechanical Properties Metric English Comments
Fatigue Strength 55.2 MPa
8000 psi
notched
ATI Wah Chang Zircadyne® Alloy Zr 705
Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other ..