Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 376 MPa | 54500 psi | Smooth, Kt=1 |
TIMET 75A CP Titanium (ASTM Grade 4) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features.. |