Polymer Property : Fatigue Strength = 50800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 350 MPa

@# of Cycles 1.00e+8
50800 psi

@# of Cycles 1.00e+8
rotating beam (Aging - 595°C/16 h F.C. to 540°C, AC)
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC..