Fatigue Strength 325 MPa
47100 psi
Limit; test specifics not reported
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties
Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v..