Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 310 - 360 MPa @# of Cycles 1.00e+8 |
45000 - 52200 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 190 Strip; HM (TM04) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R.. |
|||
Fatigue Strength | 310 - 340 MPa @# of Cycles 1.00e+8 |
45000 - 49300 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 25 Strip; HT (TH04) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 74%Superficial Hardness: 30N 58-6.. |
|||
Fatigue Strength | >= 310 MPa @# of Cycles 1.00e+7 |
>= 45000 psi @# of Cycles 1.00e+7 |
(R=-1) |
Schmolz + Bickenbach MoldMAX HH® High Hard - Copper Alloy Description: Brush Wellman’s MoldMAX HH® (High Hard) is the premier copper mold alloy. This alloy has a hardness and strength comparable with standard tool steels but its thermal conductivit.. |
|||
Fatigue Strength | >= 310 MPa @# of Cycles 1.00e+7 |
>= 45000 psi @# of Cycles 1.00e+7 |
(R=-1) |
Schmolz + Bickenbach MoldMAX LH® Low Hard - Copper Alloy Description: Brush Wellman’s MoldMAX LH® (Low Hard) is a premium copper mold alloy that provides hardness and strength comparable with standard AISI P-20 tool steel and a thermal conductivit.. |