Polymer Property : Fatigue Strength = 43500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 300 - 340 MPa

@# of Cycles 1.00e+8
43500 - 49300 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM04 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 77%Formability Ratio, 90° Bend, R..
Fatigue Strength 300 MPa
43500 psi
Limit; test specifics not reported
TIMET TIMETAL® Code 12 Titanium Alloy (ASTM Grade 12)
Features: Highly weldable, near-alpha alloy, exhibiting improved strength and temperature capability over CP combined with superior crevice corrosion resistance and excellent resistance under oxidiz..