Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 296 MPa | 43000 psi | Endurance Limit (Unnotched) |
Meehanite Ductliron® SH-100 Nodular Graphite Ductile Iron Type SP-100 is characterized by its exceptional hardenability. It is particularly suited where high strengths are desired in relatively heavy casting sections. In the as-cast condition it has a pe.. |