Polymer Property : Fatigue Strength = 42500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 293 MPa

@# of Cycles 1.00e+7
42500 psi

@# of Cycles 1.00e+7
rotating beam
Carpenter Gall-Tough PLUS™ Stainless, Annealed
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 4..
Fatigue Strength 293 MPa

@# of Cycles 1.00e+7
42500 psi

@# of Cycles 1.00e+7
rotating beam
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..