Polymer Property : Fatigue Strength = 4000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 27.6 MPa
4000 psi
Fatigue Endurance; ASTM D 671
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications
Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe..