Mechanical Properties Metric English Comments
Fatigue Strength 240 - 270 MPa

@# of Cycles 1.00e+8
34800 - 39200 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200)
Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl..