Mechanical Properties Metric English Comments
Fatigue Strength 27.0 MPa

@# of Cycles 1.00e+6
3920 psi

@# of Cycles 1.00e+6
Asahi Kasei Tenac®-C 4510 Acetal Copolymer, General Purpose  (discontinued **)
General-purpose grade, characterized by balanced flowability and mechanical properties.Applications: Gears, cams, hose joints, clips, switches, mechanical parts of audio and video equipment.This pro..