Polymer Property : Fatigue Strength = 352 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 352 MPa
51000 psi
Endurance Limit (Notched)
Meehanite K-405 Austempered Ductile Iron
Type K-405 is for applications involving wear and requiring high tensile and endurance limit. Excellent founding properties enable more accurate castings with savings in machine stock required. Da..