Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 35.0 MPa @# of Cycles 1.00e+6 |
5080 psi @# of Cycles 1.00e+6 |
1 Hz |
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |