Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Fatigue Strength = 310 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 174 Strip; 1/2HT (TH02) Temper (UNS C17410)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 190 Strip; AM (TM00) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200)
Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM00 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 25 Strip; 1/4HT (TH01) Temper (UNS C17200)
Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6..
Copyright © lookpolymers.com All Rights Reserved