Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Fatigue Strength = 29000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 200 MPa

@# of Cycles 5.00e+7
29000 psi

@# of Cycles 5.00e+7
Axial; R = 0.1; Extruded Bar; ASTM E466
Magnesium Elektron Elektron® 675 Magnesium Wrought Alloy
High strength wrought Mg alloy used for high performance components, including at elevated temperature. Excellent corrosion resistance and easily machined. Can be extruded, forged and hot formed. ..
Copyright © lookpolymers.com All Rights Reserved