Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 172 MPa | 25000 psi | |
Meehanite GM-60 Flake Graphite Cast Iron Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a.. |