Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 165 MPa | 23900 psi | casting |
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |