Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 138 MPa @# of Cycles 1.00e+6 |
20000 psi @# of Cycles 1.00e+6 |
R = -1, 105 ksi YS |
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Fatigue Strength | 138 MPa @# of Cycles 1.00e+8 |
20000 psi @# of Cycles 1.00e+8 |
rotating beam |
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i.. |