Mechanical Properties Metric English Comments
Fatigue Strength 124 MPa

@# of Cycles 5.00e+8
18000 psi

@# of Cycles 5.00e+8
completely reversed; R. R. Moore Machine and specimen.
Alcoa Toolrite 2011®-T3 Aluminum
Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting ..
Fatigue Strength 124 MPa

@# of Cycles 5.00e+8
18000 psi

@# of Cycles 5.00e+8
completely reversed; R. R. Moore Machine and specimen.
Alcoa Toolrite 2011®-T8 Aluminum
Weldability = D; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting ..
Fatigue Strength 124 MPa
18000 psi
casting
CMW® 100 Copper Alloy
CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther..