Polymer Property : Fatigue Strength = 121000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 833 MPa

@# of Cycles 1.00e+6
121000 psi

@# of Cycles 1.00e+6
Heat treatment: 1030°C, 520°C (x2), HRc63
International Mold Steel DC53 General-Purpose Cold Work Die and Mold Steel
Description: DC53 is a general-purpose cold work die and mold steel whose strength and toughness approach those of high-speed steels.Unique Characteristics: Higher hardness (62-63 HRc) than D2 after..