Polymer Property : Fatigue Strength = 10000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 68.9 MPa
10000 psi
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48
Dura-Bar G1 contains flake graphite in a matrix that is pearlitic with small amounts of ferrite. This is the softest grade of the Dura-Bar gray irons and is normally selected when excellent machinab..
Fatigue Strength 68.9 MPa
10000 psi
Dura-Bar G1A Continuously Cast Gray Iron Bar Stock ASTM A48
Dura-Bar G1A has Type D graphite in a predominantly ferrite matrix. This specification was originally developed for the glass mold industry where a fine grain structure and superior machining finish..