Mechanical Properties Metric English Comments
Notched Tensile Strength 1517 MPa

@Temperature -18.0 °C
220000 psi

@Temperature -0.400 °F
K<sub>t</sub> = 10
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Notched Tensile Strength 1517 MPa

@Temperature -184 °C
220000 psi

@Temperature -299 °F
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..