Mechanical Properties Metric English Comments
Ball Indentation Hardness 74.0 MPa

@Load 36.5 kg
10700 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MCS Polyamide 6 - Colored
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For colored parts produced by injection molding.Tarnamid® has the following ..