Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 10.2 kN/m @Temperature 60.0 °C, Time 605000 sec |
58.0 pli @Temperature 140 °F, Time 168 hour |
JRF/SW, Alclad; AMS-S83318 |
3M AC-250 B-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read.. |