Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 5.96 kN/m @Temperature 83.0 °C |
34.0 pli @Temperature 181 °F |
180° T-Peel, Etched Al/Etched Al |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |