Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 7.71 kN/m @Temperature 24.0 °C, Time 1.81e+6 sec |
44.0 pli @Temperature 75.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4475 Industrial Adhesive Features: Dries quickly to a firm bondExcellent resistance to water, plasticizer migration, many detergent and soap solutions, oils and greasesA general purpose adhesive for bonding most vinyls, cer.. |