Polymer Property : Peel Strength = 26.3 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 26.3 kN/m

@Temperature 127 °C
150 pli

@Temperature 261 °F
resistance to glass with primer; ASTM D3167
Huntsman KRYSTALFLEX® PE 192 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Peel Strength 26.3 kN/m

@Temperature 113 °C
150 pli

@Temperature 235 °F
resistance to glass with primer; ASTM D3167
Huntsman KRYSTALFLEX® PE 193 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers